Skip to content
Stains and dyesStain

CPH22/1

CPH22/1 Water-based pigment stain, light walnut

Water-reducible pigment stain, light walnut (CPH22 variant). Evens colour, hides defects, lightfast.

  • Colouring furniture in any wood species
  • Evening out colour in solid wood and veneer
  • Tinting exterior coatings (per catalog)

Mix calculator

g
Thinner700.0 %

When: The catalog gives 400–1000 % water for the CPH series; more water = lighter tone.

Additive

Ratio 100 : 700.0

ComponentWeigh out
CPH22/1part A62.5 g
WATERThinner438 g
Total500 g

Covers roughly 5.56 m² at 90 g/m².

Pot life of the mix: n/a (1K).

Ask about CPH22/1

Answers are based on the CPH22/1 data and the products it mixes with.

Questions and answers are stored to improve the assistant and prevent abuse; the question text is processed by Anthropic (USA). Privacy policy

Mixing matrix

  • WATERThinner
    % by weight: 400–600 %recommended% by volume: 400–600 %recommended

    Standard working stain.

    More water = lighter tone. Use clean, ideally filtered/demineralised water. Dilution borrowed from CPH22; if CPH22/1 is ready-to-use, add no water. Test panel first.

  • WATERThinner
    % by weight: 400–1000 %catalog

    The catalog gives 400–1000 % water for the CPH series; more water = lighter tone.

  • CFH1Additive
    % by weight: 0–200 %recommended% by volume: 0–200 %recommended

    Binder: lays down more evenly, raises less grain, locks the pigment in.

    Official (for CPH22): 0–200 % per 100 parts concentrate. The dealer says CFH1 (15–20 %) is already added to the stain — check with your batch.

  • CFH1Additive
    % by weight: 10–20 %dealer

    For better levelling of the colour.

  • CPH1 / CPH3 / CPH9 / CPH10 / CPH21 / CPH24 / CPH25 / CPH26Additive
    % by weight: any ratio %dealer

    All CPH stains intermix in any ratio to hit a target colour.

Percentages are per 100 parts of component A.

Characteristics

Lightfastness
good lightfastnessdealer
Drying · Sand or stack
4 hdealer
Drying · Conditions
20 °C
Pot life
n/a (1K)recommended
Components
1Krecommended

Colours

  • CPH22/1 · Light walnut

Application

HVLP

Pressure · fluid
gravity cuprecommended
Consumption
80–100 g/m²dealer
Recoat
4 h at 20 °C before primer/sealerdealer
Sanding between coats
Do not sand the stain itself — the pigment cuts through to bare wood instantly. Knock down raised grain only after the first sealer coat (P280–P320).recommended

Full fan, 50 % overlap, keep moving — stopping makes dark blotches. Stir before and during use; the pigment settles.

Conventional spray

Consumption
80–100 g/m²dealer

Airmix (air-assisted airless)

Consumption
80–100 g/m²catalog

For production panel work.

Cloth or pad

Consumption
80–100 g/m²catalog

Spray, then wipe straight away with a rag along the grain — evens the colour and pops the figure.

Roller

Consumption
10–20 g/m²catalog

Roller-coater line, flat panels only.

Airless

Dip or flowcoat

Process and compatibility

Substrate preparation
Sand P150–P180; for a water stain, pre-wet, dry and fine-sand to knock off the raised grain. Remove all dust.source
Goes over
bare wood
Goes under
HTL20 SM
Sanding
Before: P150, P180. After first sealer coat: P280, P320.dealer
Temperature and humidity
18–25 °C, 50–70 % RH; cold/humid = longer than 4 h.recommended
Don'ts
  • Don't sand the stain coat.
  • Don't seal before 4 h at 20 °C.
  • Don't use a mild-steel cup/gun — it's water-based.
  • Don't let it freeze.

Storage

Packaging
1 kg,5 kg,25 kgdealer
Storage temperature
do not freezerecommended

Mixed into

CPH23/1

Sources

Value tags: “official”, “dealer”, “catalog”, “schedule” are Technocolor data; “workshop” is from our own datasheets; “recommended” is our engineering estimate (hover to see the reasoning).

Not covered by the sources
  • no official page
  • exact relation to CPH22 (pre-diluted? different shade only?)
  • dilution ratio for this code
  • solids_pct
  • viscosity
  • density
  • full drying time
  • shelf life
  • safety data
  • no TDS PDF found