PPS50277
PPS50277 white thixotropic high-solids PU primer
Two-pack white high-solids polyurethane primer with the strongest thixotropy in the range. Won't run off edges, hides and fills grain well, builds hardness fast. Good for intricate carved work. Cured with PC20 at 30 % by weight (alternative PC72 at 20 %: more flexible, slower drying), thinned with S50.
- vertical surfaces
- cots and chairs in various woods
- MDF
- assembled pieces
- intricate carved work
- base under coloured enamels
- base for the 'Chrome' and 'Pearl' special effects
Mix calculator
Ask about PPS50277
Answers are based on the PPS50277 data and the products it mixes with.
Mixing matrix
- PC20Hardener% by weight: 30 %dealer% by volume: 45 %dealer
standard hardener
Fixed ratio. Don't confuse it with PPS50 (that one is 50 %).
- PC21Hardener% by weight: 30 %workshop
alternative to PC20 per the owner's datasheet
PC21 appears only in the owner's datasheet (PC20/PC21 30 %); not on the sites or in the catalogue.
- PC72Hardener% by weight: 20 %dealer
when a more flexible film is needed
Dealer prints 'С72'; the catalogue chart shows it as PC72 (aromatic, slow/flexible). More flexible film, longer drying.
- S50Thinner% by weight: 10–20 (typ. 15) %dealer% by volume: 15–35 %dealer
default; go to 20 % if you are stuck with a 1.5 mm gun
Doesn't change cure time.
- S80Thinner% by weight: 10–20 %recommended
heat above ~25 °C
Not listed by Technocolor.
| Role | Material | % by weight | % by volume | When |
|---|---|---|---|---|
| Hardener | PC20 | 30 %dealer | 45 %dealer | standard hardenerFixed ratio. Don't confuse it with PPS50 (that one is 50 %). |
| Hardener | PC21 | 30 %workshop | — | alternative to PC20 per the owner's datasheetPC21 appears only in the owner's datasheet (PC20/PC21 30 %); not on the sites or in the catalogue. |
| Hardener | PC72 | 20 %dealer | — | when a more flexible film is neededDealer prints 'С72'; the catalogue chart shows it as PC72 (aromatic, slow/flexible). More flexible film, longer drying. |
| Thinner | S50 | 10–20 (typ. 15) %dealer | 15–35 %dealer | default; go to 20 % if you are stuck with a 1.5 mm gunDoesn't change cure time. |
| Thinner | S80 | 10–20 %recommended | — | heat above ~25 °CNot listed by Technocolor. |
Percentages are per 100 parts of component A.
Characteristics
- Solids
- 72 ± 1 %dealer
- Mixed solids %
- ≈ 56 %recommended
- Viscosity
- 12-13 Pa·sworkshop
- Density · Part A
- ≈ 1.5 g/mlrecommended
- Density · Mixed
- ≈ 1.3 g/mlrecommended
- Pot life
- 3–4 hdealer
- Drying · Dust-free
- 40workshop
- Drying · Touch-dry
- 40dealer
- Drying · Sand or stack
- 8 (overnight is safer) hrecommended
- Drying · Full cure
- 8dealer
- Drying · Conditions
- 20 °C
- Thixotropy
- yescatalog
- Hiding power
- highdealer
- Hardness
- builds hardness fast, high strengthcatalog
- Elasticity
- higher with PC72 instead of PC20dealer
Colours
- white · white
Application
HVLP
- Nozzle
- 1.8–2 mmworkshop
- Pressure · air
- 2–2.5 barrecommended
- Spray viscosity
- 24–30 s DIN4recommended
- Consumption
- 120–150 g/m²catalog
- Wet film
- 95–120 µmrecommended
- Coats
- 1–2 coatsrecommended
- Flash-off
- 10–20 minrecommended
- Recoat
- wet-on-wet after 10-20 min, or after full dry (8 h) and sandingrecommended
- Sanding between coats
- 280–320 grit Precommended
1.8-2.0 mm tip. Good on carving and edges - it won't run.
Conventional spray
- Nozzle
- 1.8–2 mmrecommended
- Pressure · air
- 3–4 barrecommended
- Consumption
- 120–150 g/m²catalog
Airmix (air-assisted airless)
- Nozzle
- 0.28–0.33 mmrecommended
- Pressure · fluid
- 60–100 barrecommended
- Pressure · air
- 1–2 barofficial
Not listed by Technocolor.
Airless
- Nozzle
- 0.33–0.38 mmrecommended
- Pressure · fluid
- 140–190 barrecommended
Not listed by Technocolor; levels poorly on flats.
Process and compatibility
- Substrate preparation
- MDF: P180-P220, edges P240. Solid wood: P150-P180. Moisture 8-12 %.recommended
- Goes over
- bare MDF / bare solid wood
- Goes under
- coloured PU enamels (RAL) / RAL 9005 enamel (Chrome effect)
- Sanding
- 280–320 grit Precommended
- Don'ts
- don't use PPS50's 50 % hardener dose - this one is 30 %
- don't sand before 8 h
- don't shoot it through 1.5 mm without thinning to 20 %
Storage
- Packaging
- 1,5,25 kgdealer
Mixed into
Sources
Value tags: “official”, “dealer”, “catalog”, “schedule” are Technocolor data; “workshop” is from our own datasheets; “recommended” is our engineering estimate (hover to see the reasoning).
- dealer: PC20 30/45, S50 10-20/15-35, alt C72 20 %, solids 72±1, pot life 3-4 h, touch 40 min, full 8 h, packs 1/5/25 kg
- second dealer (woodonline), same mixing table and data
Not covered by the sources
- no official t-color.ru page for PPS50277
- dealer viscosity printed as '36-3,5 Па*с' (garbled); only owner's 12-13 Pa·s is usable
- solids 72 ± 1 % (dealer) vs 73 % (catalogue, owner)
- PC72 and PC21 volume ratios unknown
- electrostatic suitability not stated
- shelf life, storage temperature
- density (only derived)
- hardness / chemical resistance numbers
- no Technocolor TDS PDF found