APL70 R9010 M
Acrylic touch-up enamel aerosol, RAL 9010 Pure White (20 gloss)
Acrylic enamel in a spray can for touch-up and repair work, tinted to RAL 9010 Pure White, satin-matt 20 gloss. Ready to use — nothing to add, nothing to thin. Good hiding, rich colour, fast drying, and it leaves no overspray halo around the repair. Comes with two caps: one for halo-free spot repairs, one for general coating.
- any wood species
- first-time finishing of small parts
- restoring the finish after a defect has been repaired (chips, scratches, dents)
- evening out the sheen over a repaired spot
- touching up white furniture and fronts in RAL 9010
Single-component product: no mixing needed — use as supplied (see application below).
Ask about APL70 R9010 M
Answers are based on the APL70 R9010 M data and the products it mixes with.
Characteristics
- Solids
- ≈ 15–25 (готовая аэрозольная смесь, с пропеллентом)recommended
- Viscosity
- n/arecommended
- Gloss
- 20 глосс (GU 60°)dealer
- Drying · Touch-dry
- 10–20dealer
- Drying · Full cure
- 3–4dealer
- Drying · Recoat (min)
- 5–10 between light coatsrecommended
- Drying · Sand or handle (h)
- ≥ 4; полировать/лишний раз трогать — через 24 чrecommended
- Drying · Conditions
- 20 °C
- Pot life
- n/arecommended
- Hiding
- high hiding powerdealer
- Lightfastness
- не желтеет в интерьере (ожидаемо)recommended
Colours
- RAL 9010 · Pure White
Application
Conventional spray
- Device
- aerosol_can
- Nozzle
- заводские насадки баллона (2 шт.); размер не указываетсяrecommended
- Pressure · fluid
- ≈ 3–5 (внутреннее давление баллона при 20 °C)recommended
- Pressure · air
- n/arecommended
- Spray viscosity
- not adjustablerecommended
- Gun distance
- 15–25dealer
- Consumption
- 80–100dealer
- Consumption, catalogue (g/m²)
- 150catalog
- Coverage per can (m²)
- ≈ 2–3 м² на баллон за один проходrecommended
- Coats
- 2–3 лёгких слоя вместо одного толстогоrecommended
- Flash-off
- 5–10recommended
- Recoat
- 5–10 мин между слоями; после полного высыхания (3–4 ч) — только по лёгкой шлифовкеrecommended
- Sanding between coats
- между лёгкими слоями не нужна; при пыли — подшлифовать P800–P1000 после полного высыханияrecommended
Shake the can well before use (typically 1–2 min after the ball starts rattling).; Do not spray onto cold or hot surfaces.; Hold the can 15–25 cm from the surface.; When done, turn the can upside down and spray until only clear gas comes out to clear the nozzle. dealer
Process and compatibility
- Substrate preparation
- Works on any wood. Fix the defect first (fill/sand), then paint; degrease the surrounding old finish and scuff it with P400–P600 so the enamel bites.recommended
- Sanding
- перед покраской — P400–P600 по старому покрытию; по финишу — не шлифоватьrecommended
- Temperature and humidity
- 18–25 °C, отн. влажность ≤ 70 %; баллон и деталь — комнатной температурыrecommended
- Don'ts
- Do not spray onto cold or hot surfaces.
- Do not lay it on in one heavy pass — it will run.
- Do not try to add hardener or thinner — it's a ready aerosol.
- Do not leave the cap unpurged after use.
Storage
- Packaging
- 400 мл аэрозольный баллонdealer
- Tint to order
- белая APL70 колеруется в любой цвет под заказ партией от 24 шт.catalog
- Storage temperature
- +5…+25 °C, вдали от солнца и нагрева, не выше +50 °Crecommended
Safety: Pressurised, highly flammable aerosol: keep below +50 °C, do not pierce or burn even when empty, never spray near a flame. Work with ventilation, wear an A-type (organic vapour) respirator and gloves.
Sources
Value tags: “official”, “dealer”, “catalog”, “schedule” are Technocolor data; “workshop” is from our own datasheets; “recommended” is our engineering estimate (hover to see the reasoning).
- dealer page: description, properties, use, 80–100 g/m², 15–25 cm, full dry 3–4 h, gloss 20, 400 ml, RAL9010, price
- sister APL70 SM: touch dry 10–20 min
- sister APL70 M: family description, 2 nozzles, hiding
- official methods page (no aerosol section; spray guidance generic)
Not covered by the sources
- официальная страница t-color.ru отсутствует
- технический лист (ТДС) и паспорт безопасности APL70 не найдены
- сухой остаток, плотность, состав пропеллента не опубликованы
- время сушки на ощупь для R9010 не указано (взято с APL70 SM)
- срок годности не опубликован
- расход: расхождение дилер 80–100 г/м² vs каталог 150 г/м²
- APL70 не входит ни в одну официальную схему отделки (information/technology)